Table 2 Mean and standard deviation of before and after in both groups and comparison between both groups (effect of material)

From: Effect of thermocycling on acetal resin versus PEEK surface hardness and flexure strength of implant-retained overdenture bars: in vitro study

 

PEEK

Acetal

P value

M

SD

M

SD

Before

26.30

0.14

23.63

0.93

0.0001*

After

24.50

0.20

21.03

0.21

0.0001*