Table 1 Labelling of samples based on different milling hours and annealed temperature

From: Applicability of carbothermic reduction for upgrading Sri Lankan ilmenite ores: towards converting ilmenite into synthetic rutile by mechanical activation

Annealed temperature (°C)

Milling hours

1 h

2 h

3 h

4 h

1200 °C

M1/1200

M2/1200

M3/1200

M4/1200

1100 °C

M1/1100

M2/1100

M3/1100

M4/1100

1000 °C

M1/1000

M2/1000

M3/1000

M4/1000

900 °C

M1/900

M2/900

M3/900

M4/900

800 °C

M1/800

M2/800

M3/800

M4/800