Table 5 Measurements of thin film thickness after electrolytic coloring of Al samples

From: Electrodeposition of nano-Cu, Ni and binary Ni/Cu into nano-porous AAO layer for high-efficiency black spectrally selective coating

Sample

Anodization time (min)

Thickness (μm)

Al blank

1

Al anodized

30

15

Al colored by Ni

30

16

Al colored by mixture Ni and Cu

30

10

Al colored by Cu

20

8

Al colored by Cu

30

11

Al colored by Cu

60

20