Fig. 6From: Electrodeposition of nano-Cu, Ni and binary Ni/Cu into nano-porous AAO layer for high-efficiency black spectrally selective coatingDetermination of Cu content (mg/cm2) of electrolytically colored Al samples at different anodization time of 20, 30 and 60 minBack to article page