From: Re-mineralization potential, shear bond strength and hydration characteristics of experimentally prepared tri-calcium aluminate phase-modified glass ionomer cement on sound and caries-affected dentin (An in vitro/in vivo study)
Ingredients
Concentration (g/L)
NaCL
0.4
KCl
0.48
CaCl2·2H2O
0.795
Na2S H2O
0.005
NaH2PO4 2H2O
0.78
Urea
1
Phosphoric acid to adjust pH to 6.4