Skip to main content

Table 5 Some properties of W0, WSG1, WSG2 and WSG3 samples sintered at 900 °C/2h

From: Trials of reuse the Pb-containing wastes of crystal glass factories into useable new materials

Sample NoPhysical PropertiesNature of the ProductPhoto
Density
g/cc
±0.005
Compression strength
KN/mm2
±0.1
Porosity
%
±1
W00.39210.2630.19Ceramic material : Yellowish green with very porous
WSG12.50931.169.81Ceramic material : light yellowish green
WSG22.73215.169.33Ceramic material : light whitish green
WSG32.74383.2514.02Ceramic material : light green