Table 4 EDX microanalysis of W0 and WSG2 samples sintered at 900 °C/2 h

From: Trials of reuse the Pb-containing wastes of crystal glass factories into useable new materials

 EDX microanalysis
ElementsW0/wt.%WSG2/wt.%
O19,4032.62
F1.331.30
Si26.6335.76
Al0.320.68
Na1.655.53
K4.423.40
Ca4.373.34
La3.47
Ce4.15
Fe5.313.88
Pb28.9413.51