Fig. 12
From: To blend is a good solution to improve the heat insulation applicability of diatomite ores

XRD analysis of M2-D2 (30/70% mass) specimens fired at 1100 °C for 1 h
From: To blend is a good solution to improve the heat insulation applicability of diatomite ores
XRD analysis of M2-D2 (30/70% mass) specimens fired at 1100 °C for 1 h